Investment Casting

  • Analysis and solution of common problems in casting wax mould

  • 1、Wax mould surface is not smooth

    Reason

    Solution

    Wax temperature too low

    Change the wax temperature and increase the wax temperature appropriately

    Wax injection pressure is too low

    Increase wax injection pressure

    Mold temperature is too low

    Reduce the amount of cooling ice

    Insufficient wax flow rate

    Increase the flow rate of wax during wax injection

    The mould surface is too roughMake the mould surface as smooth as possible
    Too much mold releaseReduce the use of release agents

    2、Wax mould burst

    Reasons for the formationImprovement method and description
    Hold time is too longReduce the holding time, before the wax has been cold set, still toughness but not hard brittle, remove the wax from the self-mold.
    Improper mold opening and wax removalThe mold should be opened in sequence, and the wax embryo should be taken with care, not too much force.